This welding heat input calculator works out the heat put into a joint for a welding procedure record. Enter the arc voltage, current and travel speed — or the run length and arc time — and choose the process, and it shows the arc energy, the heat input with the process's thermal efficiency, and the travel speed, in kJ/mm and kJ/in. Paste every pass of a procedure qualification to check them against your WPS limits. It runs in your browser.
| Volts | Amps | mm/min | k | Arc energy | Heat input |
|---|---|---|---|---|---|
| 22 | 100 | 150 | 0.6 | 0.88 | 0.53 |
| 24 | 140 | 200 | 0.8 | 1.01 | 0.81 |
| 26 | 220 | 300 | 0.8 | 1.14 | 0.92 |
| 30 | 600 | 500 | 1.0 | 2.16 | 2.16 |
Volts × amps × 60 ÷ (1,000 × travel speed in mm/min) gives kJ/mm of arc energy; multiply by the process efficiency for heat input.
EN 1011-1 uses 1.0 for SAW, 0.8 for MMA, MIG/MAG and FCAW, and 0.6 for TIG and plasma.
ASME IX uses arc energy without the factor; check what your code and WPS require.
Run length ÷ arc time × 60 gives mm/min.
No. Everything runs in your browser.
Arc energy (kJ/mm) = voltage × current × 60 ÷ (1,000 × travel speed in mm/min). Heat input = arc energy × the thermal efficiency factor k from EN 1011-1 (submerged arc 1.0; manual metal arc, MIG/MAG and flux-cored 0.8; TIG and plasma 0.6). Travel speed can be entered directly or from run length ÷ arc time. Results are also given in kJ/in. Batch mode reads each pass of a procedure.